TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vgcFK-0000UNC; Sat, 4 Jan 97 13:59 CST
Old-Return-Path:
Date:
Sat, 4 Jan 1997 15:08:24 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/8968
TO:
From [log in to unmask] Mon Jan 6 10:
33:01 1997
Resent-Message-ID:
<"oRhNU2.0.5t7.DQhpo"@ipc>
Subject:
From:
Return-Path:
<TechNet-request>
X-Loop:
Message-ID:
Parts/Attachments:
text/plain (17 lines)
A few years ago I plated a bunch of boards wirh all tin for an OEM who
built product with them.  A "short" time thereafter, the product all bombed
out from shorts created by tendrites of tin.  The OEM was embarassed,
out a lot of money and learned their lesson.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2