Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vnpz4-0000kmC; Fri, 24 Jan 97 12:04 CST |
Encoding: |
1634 Text |
Old-Return-Path: |
|
Date: |
Fri, 24 Jan 97 08:27:29 EST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"OM3wa1.0.Dp2.TcFwo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Message-Id: |
|
From [log in to unmask] Fri Jan 24 12: |
05:34 1997 |
Parts/Attachments: |
|
|
TA Gaylor:
You might want to contact Advanced Plasma Systems in St. Pete, FL or
look at their web page. Very knowledgeable people.
http://www.advancedplasma.com/20fa.html
Regards,
Ron Yanuszewski
______________________________ Reply Separator _________________________________
Subject: Plasma
Author: [log in to unmask] at !INTERNET
Date: 1/24/97 12:45 AM
I am interested in the Plasma desmear process. I have been reading alot
about this type of desmear technique and dont quite understand the
variables involved.
>From what I understand there is a combination of three gasses that
combine to create the "plasma" state ( the most common oxygen, nitrogen
and tetraflouromethane).
How are these gasses controlled and what effects do the ratio of the
gasses effect the etchrate?
T.A. Gaylor
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|