HI
I know that some of you out there are having excellant results using the Morton
MX series photo resist for pattern plating. I am experimenting with this
material and I to have resolved some remarkably small and difficult patterns.
But I need some advise that the Morton rep's can't seem to give me. How do you
guys strip this stuff. I use Alkastrip AQI in my stripper (Monoethanolamine) at
7% at 120 F. for the regular resist. I have tried raising the concentration to
10% and the temperature up to 132 F. and there is still resist. I tried 5 %
NaOH at 125 F., this improved the situation but there is still some residual
resist on these panels.
I will appreciate any thoughts. Thanks in advance.
Chuck Brummer
Acuson
(818) 734-4930
[log in to unmask]
have you talked to Ken Bridges from Morton? He is the resident expert
I have worked with him many times in the past.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************