TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vkXKz-0000TWC; Wed, 15 Jan 97 09:33 CST
Old-Return-Path:
Date:
Wed, 15 Jan 1997 08:55:35 +600 CDT
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
Priority:
normal
From [log in to unmask] Wed Jan 15 15:
05:33 1997
TO:
X-Confirm-Reading-To:
"Luis Rivera" <[log in to unmask]>
X-Loop:
X-Mailing-List:
<[log in to unmask]> archive/latest/9233
Resent-Message-ID:
<"Qhk_q.0.0pF.tYFto"@ipc>
Subject:
From:
"Luis Rivera" <[log in to unmask]>
Return-Path:
<TechNet-request>
X-Mailer:
Pegasus Mail v3.40
Organization:
CompuRoute, Inc.
Message-Id:
Parts/Attachments:
text/plain (76 lines)

This E-Mail addresses the section of Doug Paul's response to Ellen 
Bekrman that mentions the Labeling Law.

Ellen, the EPA established a hotline in early 1993 when the labeling 
law went into effect, it is (800) 296-1996. I just called the number 
and it is still active. 

Please feel free to contact me directly if there is interest in 
knowing how we and many of our customers responded to the labeling 
regulation (40 CFR Part 82 - Protection of Stratospheric Ozone).

Best regards,

Luis Rivera
CompuRoute, Inc.
Dallas, TX
[log in to unmask]
(214) 340-0543



> From: [log in to unmask]
> Date: Tue, 14 Jan 1997 16:00:32 -0500 (EST)
> Message-Id: <[log in to unmask]>
> To: [log in to unmask]
> Subject: Re: cleaners for RMA flux
> 
> <<  For those of you who still use RMA flux - what are you using to clean
> your 
>  boards?  Should boards being cleaned with HCFCs be labelled (Montreal 
>  Protocol)?
>   
>  Ellen Berkman
>  Excalibur Systems >>
> 
> Ellen,
> Our lab deals with a wide variety of processes, including low solids, water
> solubles, and traditional high solids RMAs, usually from a residue
> standpoint.  There are still a wide variety of processes being used and a
> number of manufacturers are remaining with high solids RMAs, due to the
> protection afforded by all that rosin.  Most of the customers that we deal
> with who are still using HCFCs are looking to get out of them quickly.  The
> increasingly hard line taken by the EPA on HCFCs makes this a very
> unattractive option.  You would have to contact the EPA to determine if HCFC
> cleaned assemblies are included in the CFC Labelling Law.  Perhaps another
> individual on this forum could comment on that aspect.  I don't deal with the
> Labelling Law much.

A segment of Doug's response E-Mail was left out for brevity purposes.

Luis 

> 
> 
> Doug Pauls
> Technical Director
> Contamination Studies Labs
> [log in to unmask]
> (317) 457-8095
> EIEIO
> 
 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2