We use Alpha Metals Fine Line 2000 (62/36/2, RMA) solder paste.
Who has experience with cleaning this no-clean paste after reflow ?
Any residue is NOT acceptable.
Is there an ideal (aqueous) cleaning method (machine/saponifier/parameters) ?
Thanks for your input !
***********************************