In a message dated 96-11-18 12:07:56 EST, you write:

>What chemicals would you use to remove SnPb Oxidation?
>     

A strongly chelated, alkaline cleaner, buffered to insure that you do not
attack the Tin works very well.  Incidently, this is a good description of
"Cascade", see discussion of some weeks ago.....

Rudy Sedlak

***************************************************************************