Subject: | |
From: | |
Date: | 23 Oct 96 15:33 GMT+0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Date : 23/10/96 11:38
Msg From: PROCESS ENGINEERING
hello
is there any criterion for baking of HASL PCBs . actually as per
customers guidelines we have to bake the HASL pcbs prior to their use
in assembly line. kindly suggest any standard or general practice
i.e. the temperature & the duration for which the pcbs should be
baked.
if baked pcbs are to be used after a gap of a day or a week, should
they be baked again? or they can be stored in controlled envoirnment
kindly comment
regards
nalin
altos india limited
e-mail<[log in to unmask]>
e-mail<[log in to unmask]>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************