Hi,
Would like to know if there is any recommendation on printing solder paste onto
exposed solder pads which the solder mask over bare copper is 3 mils higher than
the exposed solder pads? Recently, we are attempting to print so but result in
solder shorts due to extra heights.
Appreciate any helpful info.