You might check into the possibility of induction soldering.  I have seen
that used with good success on some connector asseblies (both planar and
pth), but don't recall whether paste or preforms were used.  Jim Moffitt/EMPF


At 08:00 AM 8/6/96 -0500, you wrote:
>-- [ From: Jim Zanolli * EMC.Ver #2.10P ] --
>
>Does anyone have any ideas on how to solder thru-hole connectors
>without the extra step of wave soldering? In many cases a sufficient
>volume of solder cannot be achieved by applying solder paste to the
>hole. 
>
>In another case the connector has long .485" .025 square tails that
>must have  gold plating to allow mating to another connector after
>soldered to PCB -- and therefore cannot even be wave soldered. Are
>there any alternatives to laborious hand soldering or solder donuts?
>
>Does the term "intrusive reflow" define the soldering of thru-hole
>leads by paste in the hole and reflow?
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2