Anyone pre-baking prior to the wave with OSP on the boards. Time and
Temp? Seems I heard about an oxidation of the Cu under the OSP, or
was the T & T too much? Question comes up because of the necessity to
bake things such as Thermount boards prior to any temp. stressing.
Thanks, Neal Preimesberger, HMSC Tucson. 520-794-1030
[log in to unmask]
|
|
|