Date : 15/5/96 18:11
Msg From: ATUL RASTOGI
The shelf life of OSP boards is 6 months in vacuum sealed packs.You
can store these boards from a RH ranging from 30% to 70% without any
deterioration in the shelf life as long as vacuum seal is intact
Atul Rastogi
>>>>>>>>>>>>>>>
Posted: Tue, May 14, 1996 11:25 PM Msg:
BJJG-2076-4363/20
From: ("RFC-822": <TechNet-request(a)ipc.org>, SITE:INTERNET)
To: ("RFC-822": <technet(a)ipc.org>,SITE:INTERNET)
CC: AIL.EHTP/PCL
Subj: ASS: Storeage of PWB
RFC-822-Headers:
Resent-Date: Tue, 14 May 1996 06:41:27 -0700
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Encoding: 6 TEXT
X-Mailer: Microsoft Mail V3.0
Resent-Message-ID: <"jUSfb1.0.iu6.In6cn"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/4112
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
What is the shelf life of Copper bare boards with OSP finish.
What is the nominal RH at which the board may be stored at.
If it's 45% RH, what's the effect if environment RH is increased to
60%
ie what effect will an increase of RH have on the PWB during
storeage?
Thanks in advance.
<<<<<<<<<<<<<<<
|
|
|