I'm a pcb designer. I have a customer that needs the option of using either
a .3 wide or .4 wide 32 pin j-leaded part in the same location.
These are only prototype boards and small quantity. Probably won't be reflowed.
Question:
In order to accomodate both parts the footprint is going to be extra long.
What problems will be encountered soldering the part to the board? Will the
solder wickup onto the j-lead properly?
Any suggestions?
--------------------------------------
Larry L. Pucket
Sandia National Labs.
Dept. 9784 MS/0624
P.O. Box 5800
Albuquerque, NM 87185-0624
Email: [log in to unmask]