Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vNRiS-0000SHC; Tue, 12 Nov 96 16:54 CST |
Old-Return-Path: |
<TechNet-d-request> |
Date: |
Tue, 12 Nov 96 16:50:55 CST |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Thu Nov 14 16: |
54:19 1996 |
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"s7njx2.0.8BO.60GYo"@ipc> |
Subject: |
|
X-Priority: |
3 (Normal) |
X-Loop: |
|
Resent-Sender: |
|
From: |
|
Parts/Attachments: |
|
|
Be very careful in using galvanic potential chart.
1. The relative potential can change depending on the environment. The
most popular chart is based on metals immersed in salt water, which may not
be the same as your application condition,
2. The galvanic series shows the "thermodynamic" difference, it has no
information on the "kinetics" of corrosion. It indicates there may be a
corrosion problem, it does not tell how bad corrosion will be. If the
potential difference is large, care must be taken, or test must be
performed.
Kuan-Shaur Lei, Ph.D.
Senior Member of Technical Staff
Advanced Technology Department
Compaq Computer Corporation
[log in to unmask]
(281) 518-8099 (phone)
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|