Stephen,
I would refer to Table 3 of IPC-RB-276, amendment 1 (published 11/94), for
gold or other plating/coating thickness requirements. This is the most
recently published IPC standard for finished plating.
Mike Buetow
IPC Technical Staff
2215 Sanders Road
Northbrook, IL 60062
P: 847-509-9700, ext. 335
F: 847-509-9798
[log in to unmask]
On Wed, 24 Apr 1996, Stephen Cooper wrote:
> Can anyone supply a specification to call up when requesting a Gold
> Flash finish on a PWB and is it worth it today, with the advances
> with the HASL finishes.
>
> Regards
>
> Stephen Cooper
> Manufacturing Projects Manager
> SCITEC LIMITED
> Apollo Place
> Lane Cove NSW 2066
> Australia
> PH : +612 428 9500
> Fax : +612 428 9589
> Email : [log in to unmask]
>
>
|
|
|