Hi Karl - please define what you mean by "open". Is it the solder
joint or is it the component?
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Open Diodes
Author: [log in to unmask] at ccmgw1
Date: 4/11/96 7:41 PM
We are having a problem with melf diode components being open after reflow
solder. Would using the IPC detent pattern reduce this problem?
Karl Kaylor
[log in to unmask]
(317) 587-4684
|
|
|