Another option that works quite well is using clear (unpigmented)
soldermask and covering the fiducials with the soldermask.
______________________________ Reply Separator _________________________________
Subject: RE: Exposed Copper on Assemblies
Author: [log in to unmask] at corp
Date: 2/26/96 7:48 AM
Reflowing solder paste on fiducials and in-circuit test pads shouldn't cause
any problems. We've been performing ICT on assemblies with solder on the test
pads for years. I can't speak for all, but I know that the majority of
component placement systems can read solder coated fiducials quite well.