Would appreciate any source for info on effects on solderjoint
reliability when assembling (solderpaste / IR Reflow ) a full gold
(approx 30 microinches thick) finished board. What are the effects of
the gold alloying with the tinlead in the joint ? / Thank you.
***************************************************************************