Dexter Makes a peroxide/biflouride based chemistry that is effective in
removing 63/37 tin /lead from circuit boards. The chemistry is called SS-2853.
Contact:
Dexter
Mike Monnin
206-486-8320
[log in to unmask] Wrote:
|
| I'm looking for chemistries/recipes that will be effective
| in stripping 90/10
| tin-lead alloys off of copper leadframe devices (7025 and
| 194 Cu) that will
| leave the copper intact. I don't really care what happens
| to the plastic
| packaging. I know tin and/or tin-lead is used as an etch
| resist in the PCB
| industry, whatever chemistries are in use will probably
| work for me.
|
| Thanks in advance for your responses.
|
| Tracy Tennant
| Reliability Engineer
| Micron Technology, Inc.
| [log in to unmask]
|
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using
| SmartList v3.05 *
| **********************************************************
| *****************
| * To unsubscribe from this list at any time, send a
| message to: *
| * [log in to unmask] with <subject: unsubscribe> and
| no text. *
| **********************************************************
| *****************
|
|
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|