Jim,
If you have access to the book "Surface Mount Technology: Recent Japanese
Developments,"
published by IEEE Press, 1993, there is an interesting discussion of
tombstoning in the Chapter
which begins on p 77 "Overview of Placement and Bonding Technology for 1005
Components
and 0.3mm-Pitch LSIs: An Equipment Perspective."
-------
>From: Jim Marsico
>To: technet
>Subject: TOMBSTONING
>Date: Thursday, February 08, 1996 7:20PM
>
>What are some of the major causes of tombstoning of small chip SMT
components?
>
>Jim M.
>[log in to unmask]
>
>
>
|
|
|