We are a manufacturer of solder masks. It is generally agreed that a
matte solder mask will have less solder balls with no clean fluxes. A
matte surface solder mask is also easier for inspection purposes.
>>> Barry Allen <[log in to unmask]> 08/27/96 05:51pm >>>
Greetings!
We are relatively new to the SMT assembly business. Our vendor
wants to switch from a glossy to a matte surface soldermask to
eliminate a process problem on their end. Are there any issues we
need to consider? I seem to recall a discussion about solder balls hating
matte finish.
Thanks
Barry Allen
SED Systems Inc.
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text.
*
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|