Does anyone have a working process utilizing peelable soldermask to
protect gold plated contacts during the hot air solder leveling?
We are a service shop and offer horizontal HASL as one of our
services. We currently use a HASL tape to protect the gold plate, but
we have come across a high voulme part number that has a routed slot
in the middle of the connector array. The slot extends past the
contacts and thus leaves a route for the solder to get under the tape.
This causes the tape to leak and solder to come in contact with the
gold plate causing a scrap defect.
I have tried sreenable soldermask in the past with some success. I
was never able to keep the registration tight enough to work on a part
such as this.
Any suggestions or leads to resources would be greatly appreciated.
Michael Holan
Process Engineer
Radian International
Electronics Div.
internet: [log in to unmask]
phone: 512/310-4209
fax: 512/388-0898
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|