how can you possibly say that a minimum of .0003 is required solder
works fine at .00007 thk and any coatings that are over .0003 thk tends
to dewett ref mil-p-81728a tin /lead plating spec i have been ivolved
in plating and tinning for a long time and your information is ludicrous!
***************************************************************************