If you dont specified the solder thickness on the PCB or have the incorrect land
size for the lead you will result in a low fillet. You will tend to find with
very fine pitch there will be a lack of a fillet on the toe and heel. This in
the real world.
Bob Willis
Electronic Presentation Services
2 Fourth Avenue, Chelmsford, Essex CM1 4HA. England.