Does anyone out there have experience/knowledge of mating gold-plate edge
contacts (on SIMMS - so dry contacts) with tinned connectors. Is it a no-no
from a long-term reliability point of view?
We have a first source with tinned edge contacts (matching the connector) and
are lokking at a gold-plate second source.
Terry Davey [log in to unmask]
|
|
|