I don't know of any design patterns for carbon inks.
A concern is placement, due to the electrical characteristics of the carbon.
IPC-D-275, para. 5.5.3, specifies that conductive marking inks shall be
permanent and isolated by spacing or coating from the balance of the
circuitry.