Does anyone know of a recycling/reclamantion process/equipment which can be
used on a mixture of:
2% hydrofluoric acid
25% nitric acid
Balance Water and possibly some hydrochloric acid or sulfuric acid?
I was at a facility that uses this mixture in their plating line and
generates 5000 gallons/week as waste. They would like to recycle/reuse the
acids.
Thanks in advance,
Lisa D'Agostino
CAMP, Inc/GLMTC
4600 Prospect Ave
Cleveland, OH 44103
216-432-5190
216-361-2900 (fax)
[log in to unmask]
======== Fwd by: Scott R. Simp ========
Got this off the p2 bulletin board and thought someone out here could help.
Sorry for any cross postings.
Scott Simpson
Safety Engineer
Omni-Circuits, Inc
[log in to unmask]
**************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
**************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
**************************************************************************
* If you are having a problem with the ComplianceNet forum, please call *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
**************************************************************************