--- On Mon, 14 Apr 97 12:57:41 PDT "Fidelity Technologies Corp." <[log in to unmask]> wrote:
HELP!
I have a requirement on a PWB for Gold over Silver plating over copper clad glass epoxy board.
Several mfg have told me No due to migration problems and EPA requirements. Would someone
provide provide additional information on this. I would like to show customer why and propose
gold over nickel. Many thanks.
-------------------------------------
Name: FIDELITY TECHNOLOGIES CORPORATIO
E-mail: [log in to unmask]
Date: 4/14/97
Time: 12:57:41 PM
This message was sent by Chameleon
-------------------------------------
-----------------End of Original Message-----------------
-------------------------------------
Name: FIDELITY TECHNOLOGIES CORPORATIO
E-mail: [log in to unmask]
Date: 4/14/97
Time: 1:07:39 PM
This message was sent by Chameleon
-------------------------------------
**************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
**************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
**************************************************************************
* If you are having a problem with the ComplianceNet forum, please call *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
**************************************************************************