I am not aware of any EPA requirements that would prevent gold over
silver over copper, but I think that there may be migration problems.
On Mon, 14 Apr 1997, Fidelity Technologies Corp. wrote:
>
> --- On Mon, 14 Apr 97 12:57:41 PDT "Fidelity Technologies Corp." <[log in to unmask]> wrote:
> HELP!
> I have a requirement on a PWB for Gold over Silver plating over copper clad glass epoxy board.
> Several mfg have told me No due to migration problems and EPA requirements. Would someone
> provide provide additional information on this. I would like to show customer why and propose
> gold over nickel. Many thanks.
> -------------------------------------
> Name: FIDELITY TECHNOLOGIES CORPORATIO
> E-mail: [log in to unmask]
> Date: 4/14/97
> Time: 12:57:41 PM
>
> This message was sent by Chameleon
> -------------------------------------
>
>
> -----------------End of Original Message-----------------
>
> -------------------------------------
> Name: FIDELITY TECHNOLOGIES CORPORATIO
> E-mail: [log in to unmask]
> Date: 4/14/97
> Time: 1:07:39 PM
>
> This message was sent by Chameleon
> -------------------------------------
>
> **************************************************************************
> * The mail list is provided as a service by IPC using SmartList v3.05 *
> **************************************************************************
> * To unsubscribe from this list at any time, send a message to: *
> * [log in to unmask] with <subject: unsubscribe> and no text. *
> **************************************************************************
> * If you are having a problem with the ComplianceNet forum, please call *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> **************************************************************************
>
>
**************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
**************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
**************************************************************************
* If you are having a problem with the ComplianceNet forum, please call *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
**************************************************************************
|
|
|