Holly et al,
        There are several non-rosin based fluxes available. This company should 
check with his/her flux/solder supplier. Once they change to the non-rosin based
flux, they can then deflux the boards with hot DI water as we do.   Lee Wilmot
                                                                    HADCO Corp
                                                               [log in to unmask]
______________________________ Reply Separator _________________________________
Subject: FW: solder flux residue
Author:  [log in to unmask] at SMTPLINK-HADCO
Date:    7/3/97 6:16 PM
Dear Compliancenetters -
     
I received this message via a pollution prevention listserve to which I = 
subscribe.  Does anyone know of more environmentally benign ways to = 
remove solder residue?  I imagine that this issue has arise in the = 
electronic interconnection industry.  Please respond to me and I will = 
forward.
     
Thank you!
     
Holly Lynch
[log in to unmask]
Director of Environmental and Safety Programs, IPC
     
----------
From:  NEIL KOLWEY[SMTP:[log in to unmask]] 
Sent:  Thursday, July 03, 1997 1:36 PM
To:  [log in to unmask]
Subject:  solder flux residue
     
Some fluxes contain a "rosin" as one of the active ingredients. 
Apparently this rosin leaves a residue, which must be removed after the 
solder is applied. A small company in Colorado is currently using a = 
vapor
degreaser with perc to remove this residue. Does anyone have any 
experience with any safer alternatives?=20
************************************************************************** 
* The mail list is provided as a service by IPC using SmartList v3.05    * 
************************************************************************** 
* To unsubscribe from this list at any time, send a message to:          * 
* [log in to unmask] with <subject: unsubscribe> and no text. * 
************************************************************************** 
* If you are having a problem with the ComplianceNet forum, please call  * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]     * 
**************************************************************************
     

**************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05    *
************************************************************************** 
* To unsubscribe from this list at any time, send a message to:          *
* [log in to unmask] with <subject: unsubscribe> and no text. *
************************************************************************** 
* If you are having a problem with the ComplianceNet forum, please call  *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]     *
**************************************************************************


ATOM RSS1 RSS2