"Ubl, Scott" <[log in to unmask]> Wrote:
|
|
| I am curious, what are commonly used receiving inspection
| procedures for
| outsourced multilayer PWB's and the value of individual
| procedure.
|
| I would like to know more about what other companies
| thoughts and
| procedures are, on doing solderability tests, cross section
| analysis,
| requiring COC's and ionic contamination testing at receiving
| inspection.
| Is this analysis found to be benefiticial and identify
| defective lots?
| Basically I am looking for others to share the experiences
| they had with
| bare board inspection and ideas to optimize the effectiveness
| of the PCB
| inspection step for a high quality board.
|
|
| Thank you,
|
Hello Scott -
IPC-A-600 (Acceptability of Printed Boards, Rev E) published in August
1995 is a good reference and industrial standard for bare board
inspection.
Best Regards
Nora Xiao
Tektronix, Inc.
|
|
|