Hello Technetters,
I have some questions regarding the quality of Consumables.
1. What is "Copper mirror corrosion test" ?
2. Whether this test needs to be done for "water soluble flux"
used for wave soldering ?
3. What are the other tests which need to be done before
using the water soluble flux for wave soldering ?