I'm sure it depends on the solder type used and the temp rating rating
of the PCB. We require maximum temperatures be no higher than the temp
rating of our boards (120C). This is significantly lower than the
melting point of the eutectic solder we use (183 C) so we don't consider
the solder melting point an issue. Assuming you stay below the melting
point or plastic region ( for non eutectic solders), fatigue life is an
issue which has to do with temperature cycling rather than absolute
temperature of the solder. Werner Englemaier is an expert on that
subject. He will probably comment and want to know at what rate the
solder changes temperature and what kind of joint it is.
----------
From: [log in to unmask]
To: FMGM@rkdwgc; dcreag@rkdwgc; FASP@rkdwgc; mbernh@rkdwgc;
rreyno@rkdwgc; BRAJ@rkdwgc
Subject: ASSY. Solder joint temp
Date: Wednesday, November 20, 1996 6:46PM
Hello,
Is there any standards regulating the maximum allowed solder joint
temperature during operation?
Is there a temperature upper limit when you come into real trouble from
a solder joint
reliability aspect?
We are discussing a temperature around +90 degree C for a short period(
one hour) perhaps three
times a day, low temperature +35 to 40 degrees C.
Hans Bogren
Ericsson Telecom AB
************************************************************************
***
* TechNet mail list is provided as a service by IPC using SmartList
v3.05 *
************************************************************************
***
* To unsubscribe from this list at any time, send a message to:
*
* [log in to unmask] with <subject: unsubscribe> and no text.
*
************************************************************************
***
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|