     Try STYCAST 2850XX, from Grace Specialty; impervious to attempts at 
     mold sprue removal, using a diamond saw.


______________________________ Reply Separator _________________________________
Subject: Re: ASSY: Security coating of SMT leads.
Author:  [log in to unmask] at PMDF
Date:    11/14/96 1:57 PM


     try putting a soft fast cure rubber under the epoxy. The rubber should 
     take some of the strain.
     
______________________________ Reply Separator _________________________________
     
Subject: ASSY: Security coating of SMT leads. 
Author:  [log in to unmask] at internet
Date:    11/14/96 8:37 AM
     
     
         Another try, hopefully this time with the text itself.
     
              We will be building a product for a customer that has three
         devices that need protecting from electrical access for security 
         reasons. The customer wants a coating over the leads that will 
         prevent people from probing them to find electronic access codes 
         used in the system. Obviously this can only be a deterrent, as 
         someone sufficiently determined could get past any coating or 
         barrier.
     
              The coating needs to cover the leads only, so potting the
         entire assembly isn't on. It needs to be a fast in line process. I 
         would like to limit any off line processing, like oven curing, to 
         under one hour. The cured material needs to be resistant to 
         soldering iron heat, the sort of solvents and acids that the PCB 
         will withstand and the sort of mechanical attack that won't wreck 
         the leads.
     
              After discussion with material suppliers I can see two ways
         of doing this. One is a filled rigid epoxy material of the type 
         used for glob topping bare die, that will encapsulate the leads. 
         This will be very resistant to attempts to remove it. The Cte will 
         be closely matched to the package, lead and board materials, but 
         the elastic modulus will be high. The other group of materials are 
         of lower modulus. These however tend to be easier to remove. 
         Processing will probably be dispensing from a barrel via an X,Y,Z 
         dispensing system. Curing will either be heat, or UV.
     
              My principal concern is compromising the fatigue life of the
         solder joints by having a high modulus encapsulation material that 
         constrains the movement of the gull wing leads and puts more 
         stress on the solder joints during temperature changes. The 
         product is a relatively high value consumer item for use in the 
         home. Has anyone done something similar? What materials did you 
         use? What were the results? What was the processing like? I will 
         be doing some reliability tests, but the time constraints mean 
         that the material choice needs to be right first time.
     
              One device is a 28mm body 0.5mm pitch PQFP. The other two
         devices are smaller in size. They will be conventionally attached 
         to an FR4 board.
     
         Jeremy Drake.
         Design to Distribution Ltd. Kidsgrove, Stoke on Trent, England.
     
         +44 (0)1782 771000.
         [log in to unmask]
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************




Received: from gatekeeper.sciatl.com by ALPHA.CORP.SCIATL.COM  (PMDF V4.3-13 #7203) id <[log in to unmask]>; Thu,  14 Nov 1996 18:51:02 -0500 (EST) Received: from smap@localhost by gatekeeper.sciatl.com via smapdV1.3 id  SAA07338; Thu, 14 Nov 1996 18:53:54 -0500 Received: from ipc.org by gatekeeper.sciatl.com for <[log in to unmask]> via  SMTP (smap V1.3) id sma007305; Thu Nov 14 18:53:38 1996 Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)  id RAA09603; Thu, 14 Nov 1996 17:46:24 -0800 Received: by ipc.org (Smail3.1.28.1 #2) id m0vO8Lq-0000aDC; Thu,  14 Nov 96 14:25 CST X400-Received: by /c=us/admd=cwmail/; Relayed; 14 Nov 96 13:57:49 -0500 X400-Received: by mta MTAwltk in /c=us/admd=cwmail/; Relayed; 14 Nov 96  13:57:49 -0500 Alternate-recipient: Allowed Disclose-recipients: Prohibited Content-return: Allowed Resent-date: Thu, 14 Nov 1996 17:46:24 -0800 Date: Thu, 14 Nov 1996 13:57:49 -0500 Resent-from: [log in to unmask] From: Aric Parr <[log in to unmask]> Subject: Re: ASSY: Security coating of SMT leads. Resent-sender: [log in to unmask] Resent-sender: [log in to unmask] Resent-message-id: <"NG4cl.0.ajK.p0uYo"@ipc> Message-id:  <01680328B6BAD006*/c=us/admd=cwmail/prmd=carrier/o=syracuse/ou=ccmail1/s=Parr/g =Aric/@MHS> X-Envelope-to: "Geroux, Dick%SA-SDO"@ccmail.corp.sciatl.com,  "Jaramillo, Rick%SA-SDO"@ccmail.corp.sciatl.com,  "Webb, Doug%SA-SDO"@ccmail.corp.sciatl.com Content-identifier: 01680328B6BAD006 Content-transfer-encoding: 7BIT Conversion: Allowed Priority: non-urgent X400-Content-type: P2-1988 ( 22 ) X400-MTS-identifier: [/c=us/admd=cwmail/; 01680328B6BAD006-MTAwltk] X400-Originator: [log in to unmask] X400-Recipients: non-disclosure; Old-Return-Path: <[log in to unmask]> X-Mailing-List: <[log in to unmask]> archive/latest/7708 X-Loop: [log in to unmask] Precedence: list

ATOM RSS1 RSS2