Sometimes the cause is the CC is too thick and does not allow the
gaseous products to get out. Try thinning the CC.
______________________________ Reply Separator _________________________________
Subject: Bubbles in Conformal Coating
Author: [log in to unmask] at Internet
Date: 11/7/96 5:06 PM
I threw this question out once before but I still cannot determine the
source of bubbles in our conformal coating process. We are using an
acrylic coating and a Nordson Select Coat System. The bubbles come
and go from day to day.
We have looked at viscosity, temperature, humidity, pressure,
z-height, contamination, micro-adjust, and a few other variables. Has
anyone else seen this phenomenon or do you have any insight on it?
Any help is very much appreciated.
Thank you.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|