         An inner layer engineer would like to ask technetters the following:

1) Has anyone determined the % moisture content in inner layers, presumably
after oxide, that relates to potential delamination problems after lamination?
2) How is this moisture content measured and/or monitored?
3) What resin types (ie multifunctional, polyimide etc) are applicable?

All responses would be greatly appreciated.

Dave Rooke
Circo Craft - Pointe Claire

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2