>Specific Subject - Solid Aluminum entry material
We don't consider solid Aluminum useable for hole sizes of
0.0135" or less but this is strictly shop specific.
>4. How high would you say is the "average" drill stack for:
>a. Multilayer?
>b. Double sided?
Two high plus whatever your customer's annular ring permits.