Dear Technet;
I am currently in the process of setting up a procedure for
testing the reliability of using Single sheets of Prepreg versus
Multiple sheets of Prepreg on Multilayer Designs.
If anyone has experience with this I would appreciate any
recommendations.
You may contact me directly if necessary.
Thanks,
Nancy Nelson
Dell Computer
[log in to unmask]
or 512-728-0016
***************************************************************************