Technetters:
I'm interested in various RTVs that are approved by UL 94-V-0 for flammabil-
ity. So far I've come up with Dow Corning: 3140, 1-2577/1-2620, 838, 3145
as well as Sylgard 170 and 567. In addition, GE Silicones has its RTV133.
Is there anything else out there that can withstand operating temperatures
of at least 125 C and yet remain somewhat rubbery and pliable?
Lucy Rojao
[log in to unmask]
(416) 448-5866
***************************************************************************