Krylon is a supplier of coating materials like acrylic , it comes in a nice
easy to use spray can. Hate to say it but our factory too uses Krylon when
they mean acrylic. It is just the brand that has been in use for a long,
long time here.
----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Re: Assy: conformal coating
Date: Tuesday, September 24, 1996 1:20PM
> Try coating the whole thing with acrylic. easy to rework, negligible RF
I have become confused!
Recently, while reviewing a startup's design business, the prospect
used "conformal coat" and "Krylon" in the same sentence. I was, um,
somewhat surprised. I took the comment to be an oversimplification
from a EE's perspective.
Is the joke on me?
Thanks,
Jeff Seeger Applied CAD Knowledge Inc
Chief Technical Officer Tyngsboro, MA 01879
[log in to unmask] 508 649 9800
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|