We have done multiple DSC runs on off the shelf FR4 laminate which clearly
show that postcuring occurs. Not done it on multilayer samples (yet).

David Whalley
Loughborough University

>(1)  Is inner layer core material completely cured when it comes from the 
>supplier?  One of our guys suggested Polyclad told him that it was not - 
>that was a surprise to us, if true.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2