Sorry I forgot to mention this in my previous
submission. The operator takes 2 slugs, not 1, twice per month. One
before cleaning and one after. We have SPC charts for both. The
"before" and "after" slugs are not that much different. I can provide
data for anyone interested. Lou
.
On Mon, 5 Aug 1996 [log in to unmask] wrote:
> Joe, here are my comments about your HASL.
>
> OUr guys clean the pot once per day. The machine is only used on second
> shift.
>
> When we got a new Quicksilver machine about 2 years ago, it looks like Cu
> contamination went down, according to our SPC chart. The operators say
> it is easier to clean the new machine than the old one.
>
> We have an SPC chart to monitor Cu in the pot. On the 5th and the 20th
> of each month, the operator pulls a sample slug to be sent out for analysis.
>
> Lou Hart
>
>
> .
>
> On Mon, 5 Aug 1996, joef wrote:
>
> > Hello Technet,
> > We are having difficulty maintaining our HASL pot below 0.25% Cu, even
> > with 2x daily drossing. The machine is an old vertical Electrovert
> > with less than easy access.
> > - Is this 0.25% more critical at assembly than at fab?
> > - What is the practical USL for copper in HASL?
> > - How often should metal contaminants be measured?
> > - Should drossing be done at a constant frequency, or based on panel
> > loading?
> > - Are there any studies out there correlating HASL quality with Cu
> > contamination level?
> > - Any special recommended procedures or tools?
> >
> > As always, we appreciate any input.
> > Joe Felts
> > PC World, Toronto
> >
> > ***************************************************************************
> > * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> > ***************************************************************************
> > * To unsubscribe from this list at any time, send a message to: *
> > * [log in to unmask] with <subject: unsubscribe> and no text. *
> > ***************************************************************************
> >
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to: *
> * [log in to unmask] with <subject: unsubscribe> and no text. *
> ***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|