Subject: | |
From: | |
Date: | 02 Aug 96 09:09:16 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
You can dunk it in sulfuric acid and touch the chrome with a bar of
zinc metal or add thiourea to etch the chrome.
Aric Parr
United Technologies Electronic Controls
______________________________ Reply Separator _________________________________
Subject: Re: FAB: to etch chrome but not copper
Author: [log in to unmask] at internet
Date: 8/1/96 7:59 PM
RE: Etching chrome. As an unspecific recollection, I believe that a
KOH + Potassium Permanganate solution will strip Chrome from Copper.
I am not certain of concentrations and temperatures. Note that this
will create environmental concerns on the spent etch solution and
rinses.
Marshall Gurian
Coates ASI
______________________________ Reply Separator _________________________________
Subject: FAB: to etch chrome but not copper
Author: [log in to unmask] at internet
Date: 8/1/96 11:52 AM
Can anyone tell me what etchant will dissolve chrome but not copper?
I'm thinking about using cold dilute sulfuric acid but I'm not sure what is
used commercially anymore.
Thanks!
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|