Has anyone ever experienced a problem with bubbles in conformal
coating when using an acrylic coating (CONAP 1171) applied with a
Nordson Select Coat system? The bubbles appear instantly as the
coating is applied. The result is a non-conforming defect per
IPC-A-610 section 7.1.2. Thank you.