Electroless palladium at 6 - 8 microinches(uins) is an alternative to
selective gold, for contact switch applications.
If Pd is used as the solderability preservative in place of HASL (also 6 - 8
uins), one application will meet the requirements of both.
George Milad
Atotech USA Inc
***************************************************************************