I am in the process of having samples made with Cu/Ni/Pd/Au for gold
wire bonding. The gold in this process is immersion gold. This is
touted by two suppliers as a reliable surface for bonding. I also
have yet another supplier telling me that their electroless
nickel/electroless palladium process (NO gold) is also bondable. This
will be tested too.
I have had samples made in the past with just e-nickel and immersion
gold (which we are all experts on now) which were ball bonded with
gold wire.
I have been told that the gold wires adhered to the immersion gold
when they were new, but they won't be good for the long term. How can
I stress the deposits to determine how good my surface finishes are?
That is: How would I know if it is reliable enough for me to offer it
to MY customers?
Matt Byrne
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|