this message is being forwarded from a co-worker,
the solder joints that we are forming with our hot bar process are not meeting
the requirements of 'standard' workmanship criteria. in particular, we have a
difficult time meeting 'heel fillet' requirements. the defect is one of
'insufficient solder' at the heel fillet. it isn't that there isn't any heel
fillet; it's just that it isn't as pronounced as the standards require.
question.- are there solder joint standards specific to hot bar soldering?
thanks,
phil crepeau, trw-san diego
Judy Murray
TRW San Diego
619.592.3616
[log in to unmask]
***************************************************************************