>In response to your rusty reflow oven..
>Are you using a water cooled radiator system for you cooling zones? We do, and
>we did see a rusting problem. Particularly when we left the cooling zone
on all
>the time, even when the oven wasn't running. We were condensing water on any
>warm surface, thus rust formed.
>We got rid of the problem by keeping the water pumps off when the oven wasn't
>running. Also, our oven Manufacturer told us at one time to raise the
>temperature of the water, causing less condensation.
>