Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Tue, 31 Dec 1996 07:44:00 -0600 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Thu Jan 2 10: |
58:39 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Resent-Message-ID: |
<"JppBJ3.0._0G.weIoo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vf5em-0000U9C; Tue, 31 Dec 96 08:59 CST |
X-Mailer: |
Microsoft Exchange Server Internet Mail Connector Version 4.0.993.5 |
Message-Id: |
|
Parts/Attachments: |
|
|
We are a low volume shop that is looking to improve our product flow.
Our shop does High Mix, low quantity SMT boards. One of the ideas being
looked into is to program all the EPROM's etc on our HP 3XXX series
tester since we use a lot of the same EPROM's but different source code.
We have never done this before and we were wondering if anyone out
there is doing this and what problems they have run into?
Thanks in advance for your comments
Max Bernhardt
Woodward Governor Co.
[log in to unmask]
(970)-962-7376
fax (970)-962-7143
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|