X-mailer: |
Pegasus Mail for Win32 (v2.42a) |
Old-Return-Path: |
|
Date: |
Fri, 27 Dec 1996 10:29:05 +0000 |
Precedence: |
list |
Comments: |
Authenticated sender is <MCGARRY@[192.9.200.45]> |
Resent-Sender: |
|
From [log in to unmask] Mon Dec 30 09: |
00:46 1996 |
Status: |
O |
Priority: |
normal |
TO: |
|
X-Status: |
|
Content-transfer-encoding: |
7BIT |
X-Loop: |
|
X-Mailing-List: |
|
Resent-From: |
|
Resent-Message-ID: |
<"bY-4O.0.TZE._A0no"@ipc> |
Content-type: |
text/plain; charset=US-ASCII |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vdfma-0000UtC; Fri, 27 Dec 96 11:09 CST |
Return-Path: |
<TechNet-request> |
MIME-Version: |
1.0 |
Message-Id: |
|
Parts/Attachments: |
|
|
I AM BUILDING BOARDS OUT OF WOVEN KEVLAR MATERIAL .0045 CORE
MATERIAL USING EPOXY RESIN.
DOES ANYONE HAVE ANY INFO. ON THE SCALE FACTORS FOR THE ARTWORK FOR
THIS MATERIAL. ANY HELP WOULD BE GREATLY APPRICIATED.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|