Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vcEzG-0000YMC; Mon, 23 Dec 96 12:20 CST |
Content-Type: |
TEXT/PLAIN; CHARSET=US-ASCII |
Old-Return-Path: |
|
Date: |
Mon, 23 Dec 1996 10:29:39 -0800 (PST) |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
7BIT |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Mon Dec 23 12: |
59:32 1996 |
Resent-Message-ID: |
<"1musg1.0.P0J.jrilo"@ipc> |
Subject: |
|
From: |
|
X-Status: |
|
X-Loop: |
|
MIME-Version: |
1.0 (WebTV 1.0) |
Message-Id: |
|
Parts/Attachments: |
|
|
We have since the beginning of this problem, have changed out the
brightner lines and replaced them with new lines.As they were coated on
the inside with black (assuming fungus). The new lines were installed
inside black conduit tubing. The tubing was for the idea that the fungus
was growing from light exposure.
The size of the nodules are around .1 to .2mil, extremely small in fact,
too small too cross section and evaluate.
Sombody recommended at one time to add a small amount of copper sulfate
solution, do you have any comments on this?
T. Gaylor
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|